The NanoFab hosts UCSB Undergraduate Interns throughout the school year and summer.
The NanoFab hosts UCSB Undergraduate Interns throughout the school year and summer.

No prerequisites/prior knowledge needed; for anyone 16 years old and up; Minimum 6 months commitment (break during summer is acceptable).

* [[Nanofab Job Postings|Upcoming Internship Openings]]
* [[Process Group Interns|Current Interns]]

<br>

__TOC__


=== Internship Goals ===
=== Internship Goals ===
Line 34: Line 43:
** See the intern-generated SPC data here: [[Process Group - Process Control Data|Process Control Data]]
** See the intern-generated SPC data here: [[Process Group - Process Control Data|Process Control Data]]
* '''OCAP/Repair''': Work with tool engineers to identify & diagnose equipment problems.
* '''OCAP/Repair''': Work with tool engineers to identify & diagnose equipment problems.
** If Process Engineers identify an Out-of-Control process, Interns are involved in the communications & testing of tool repairs.
** If Process Engineers identify an Out-of-Control process, Interns are involved in the communications & testing of tool repairs, until process is back "in control".


==== Process Control for Increased Uptime ====
==== Process Control (SPC) for Increased Uptime ====
* Interns run process-control on the lab's most critical/high-usage tools.
* Interns run process-control on the lab's most critical/high-usage tools & update [[Process Group - Process Control Data|SPC charts]].
* Calibration processes are identical each time (unlike lab user's processes), allowing apples-to-apples comparisons.
* Calibration processes are identical each time (unlike lab user's processes), allowing apples-to-apples comparisons.
* Regular meetings with Process Engineers allow us to proactively identify equipment/process issues, failing tool components, and schedule repairs/remedies sooner than if detected by a lab user.
* Regular meetings with Process Engineers allow us to proactively identify equipment/process issues, failing tool components, and schedule repairs/remedies sooner than if detected by a lab user.

Latest revision as of 00:33, 11 January 2026

The NanoFab hosts UCSB Undergraduate Interns throughout the school year and summer.

No prerequisites/prior knowledge needed; for anyone 16 years old and up; Minimum 6 months commitment (break during summer is acceptable).


Internship Goals

Our goals are twofold:

  1. Increased Tool Uptime: Acquire Process Control Data so NanoFab staff can proactively identify equipment/process problems, and
  2. Industry-Relevant Experience: Give Interns hands-on industry-relevant experience to minimize the training required at any microelectronics company/research group.


The skills acquired for each goal are as follows:

Industry-relevant Experience

  • Protocols: Interns become comfortable in a busy semiconductor 'fab environment. After 2-3 months of regular usage the interns are fully comfortable with:
    • Cleanroom safety & protocols such as PPE, safe waste disposal etc.
    • Managing their own schedule to accomplish weekly processing tasks.
    • Multi-tasking to run simultaneous processes fast and efficiently.
      • Interns learn new tools only once their current cals have been condensed into a few hours.
    • Communications with
      • lab users (scheduling around other users)
      • equipment engineers (training, handling/reporting tool issues)
      • process supervisors/managers (reviewing process control data, OCAP actions)
  • Equipment: Become comfortable with learning different Operating Procedures of similar tool types
    • Eg. 4 different plasma depositions, 4 different ICP etchers etc.
    • Once an intern has learned 3 different PECVD deposition tools, it is trivial to learn a new PECVD tool even from an unfamiliar manufacturer.
  • MES: Learn to utilize production tracking/communications tools
    • Travelers/Process Followers & associated data directories are created and filled out at run-time for every calibration. (Digital/online via Google Sheets+Drive)
    • Combining Equipment Operating Procedures with Process Travelers instructions at run-time.
    • Data collection with standardized digital filenames & directory structures, available online to all lab users.
    • Click on the date of any SPC data row here to see a Traveler & Data folder filled out by interns (or here is one example).
      • Every Calibration process has the same format: see other intern-run processes here: Process Control Data
  • SPC: Perform metrology, process control, create SPC charts
    • Data from the Travelers are entered into online spreadsheets, which calculate SPC charts
    • Some interns create/modify SPC charts when needed for newly developed Cals.
    • See the intern-generated SPC data here: Process Control Data
  • OCAP/Repair: Work with tool engineers to identify & diagnose equipment problems.
    • If Process Engineers identify an Out-of-Control process, Interns are involved in the communications & testing of tool repairs, until process is back "in control".

Process Control (SPC) for Increased Uptime

  • Interns run process-control on the lab's most critical/high-usage tools & update SPC charts.
  • Calibration processes are identical each time (unlike lab user's processes), allowing apples-to-apples comparisons.
  • Regular meetings with Process Engineers allow us to proactively identify equipment/process issues, failing tool components, and schedule repairs/remedies sooner than if detected by a lab user.
  • Lab users are notified of process anomalies & repair plans, reducing bad outcomes for lab users.
  • "Contamination" checks via On-Demand process-checks
    • Determine whether a new process affects other processes on the same tool, by running pre/post Cal Etches.
    • On ICP Etchers, enables data-driven equipment sharing between processes.
    • Enables lab-users to quickly determine whether problems lie with the Equipment/"contamination", another user's process or their own Process.

Job Description: 2 phases

Internships are generally run in 2 phases, with each phase being approx. 1 Quarter (3 months) long.

Phase 1: Deposition Cals (1st Quarter)

  • Interns run 4 different deposition tools weekly, in the following order:
  • Every film undergoes the following metrology:
  • Follow Process Protocols:
    • Follow and Record Data onto Travelers for every Cal run, save metro data into publicly-accessible folders.
    • Update all SPC data tables and charts accurately, report any "out of control" process issues.
  • By the end of 1st Quarter, Interns are running 9-12 thin-film cals every 2 weeks.

Phase 2: EtchCals and LithoCals (2nd Quarter)

  • Interns run 4 different ICP Etchers weekly:
  • Metrology on each EtchCal:
    • SEM of manually Cleaved Cross-section
    • Cleaving samples for cross-sectional SEM.
    • Profilometry & Etch-Rate Calculation
    • Etch Selectivity Calculation via pre/post hardmask removal profilometry
  • Interns run weekly ASML DUV Stepper lithography: photoresist coating, exposure and develop.
    • Critical particulate-sensitive process, cal shows any particles present
      • Intern's techniques are remedied if particles are detected.
  • Metro on each LithoCal:
    • SEM for Critical Dimension measurement; multiple locations on wafer.
    • Identification of "hotspot" particulate contamination on wafer/tool.
  • Follow Process Protocols:
    • Follow and Record Data onto Travelers for every Cal run, save metro data into publicly-accessible folders.
    • Update all SPC data tables and charts accurately, report any "out of control" process issues.
  • By the end of 2nd Quarter, Interns are running LithoCals and ~2 EtchCals weekly, with multiple SEM sessions. They are proficient at SEM by the end of the 2nd quarter.