- 16:19, 5 June 2023 Ffoong talk contribs uploaded File:PPR220-7 Etch Rates (nm min) vs. Temp(C) Recipe STD O2only 3KW-3min-Temp.png
- 19:08, 2 June 2023 John d talk contribs uploaded a new version of File:PECVD1 SiN Stress vs. N2 plot.jpg (better formatting, colors axes mathcing markers etc)
- 18:52, 2 June 2023 John d talk contribs created page File:PECVD1 SiN Stress vs. N2 plot.jpg
- 18:52, 2 June 2023 John d talk contribs uploaded File:PECVD1 SiN Stress vs. N2 plot.jpg
- 03:11, 2 June 2023 John d talk contribs changed group membership for Ffoong from (none) to staff (staff user)
- 16:36, 26 May 2023 Sawyer l talk contribs uploaded a new version of File:MJB 3 IR Camera SOP Rev B.pdf
- 17:16, 24 May 2023 User account Mrsoler talk contribs was created
- 16:59, 22 May 2023 Millerski w talk contribs created page File:RTA SSI Operating Instructions.pdf
- 16:59, 22 May 2023 Millerski w talk contribs uploaded File:RTA SSI Operating Instructions.pdf
- 07:16, 20 May 2023 User account Yuxuan Xie talk contribs was created
- 23:30, 18 May 2023 John d talk contribs created page File:ASML CD Cals - Example Plot.jpg
- 23:30, 18 May 2023 John d talk contribs uploaded File:ASML CD Cals - Example Plot.jpg
- 23:28, 18 May 2023 John d talk contribs created page File:ASML CD Cals - Example Table.jpg
- 23:28, 18 May 2023 John d talk contribs uploaded File:ASML CD Cals - Example Table.jpg
- 16:04, 15 May 2023 Millerski w talk contribs created page File:Mechanical Polisher SOP Rev A.pdf
- 16:04, 15 May 2023 Millerski w talk contribs uploaded File:Mechanical Polisher SOP Rev A.pdf
- 05:05, 11 May 2023 John d talk contribs created page File:SEM1 JEOL IT800HSL.jpg (photo of SEM #1, JEOL IT800HSL)
- 05:05, 11 May 2023 John d talk contribs uploaded File:SEM1 JEOL IT800HSL.jpg (photo of SEM #1, JEOL IT800HSL)
- 04:58, 11 May 2023 John d talk contribs created page File:Amscope Stereoscope Photo.jpg
- 04:58, 11 May 2023 John d talk contribs uploaded File:Amscope Stereoscope Photo.jpg
- 04:54, 11 May 2023 John d talk contribs created page File:OlympusDSX1000.jpg (photo of Olympus DSX-1000 microscope)
- 04:54, 11 May 2023 John d talk contribs uploaded File:OlympusDSX1000.jpg (photo of Olympus DSX-1000 microscope)
- 04:51, 11 May 2023 John d talk contribs created page File:DektakXT.jpg (image of Dektak XT)
- 04:51, 11 May 2023 John d talk contribs uploaded File:DektakXT.jpg (image of Dektak XT)
- 19:34, 10 May 2023 John d talk contribs created page SEM 1 (JEOL IT800SHL) (iniital page copied from SEM2) Tag: Visual edit: Switched
- 17:34, 10 May 2023 Sawyer l talk contribs created page File:EB2 SOP Rev G.pdf
- 17:34, 10 May 2023 Sawyer l talk contribs uploaded File:EB2 SOP Rev G.pdf
- 17:00, 28 April 2023 John d talk contribs created page File:Vented font screnshot.jpg
- 17:00, 28 April 2023 John d talk contribs uploaded File:Vented font screnshot.jpg
- 16:57, 28 April 2023 John d talk contribs created page File:Vernier Template v2 screenshot.jpg
- 16:57, 28 April 2023 John d talk contribs uploaded File:Vernier Template v2 screenshot.jpg
- 16:54, 28 April 2023 John d talk contribs uploaded a new version of File:Vernier Template.gds (corrected text by flattening. Demis D John.)
- 16:51, 28 April 2023 John d talk contribs uploaded a new version of File:Vernier Template.gds (Vernier_Template_v2.gds - arrays instead of flat, and text for each layer)
- 19:44, 26 April 2023 John d talk contribs created page Ellipsometer (Woollam) - Measuring thin dielectrics with Native Oxide pre-measurement (added basic description & steps referring to for details, Measuring_thin_metals_with_oxide_pre-measurement) Tag: Visual edit
- 06:27, 26 April 2023 John d talk contribs uploaded a new version of File:IBD Schematic.jpg (added numbering for each component)
- 06:23, 26 April 2023 John d talk contribs created page File:IBD Schematic.jpg
- 06:23, 26 April 2023 John d talk contribs uploaded File:IBD Schematic.jpg
- 21:51, 17 April 2023 John d talk contribs uploaded a new version of File:Vented font DDJ.gds (added "UCSB Nnanofab" in the comments)
- 03:11, 15 April 2023 John d talk contribs created page Automated Wafer Cleaver (Loomis LSD-155LT) (initial page) Tag: Visual edit: Switched
- 15:56, 14 April 2023 John d talk contribs changed group membership for Plenvik from (none) to staff (was never set when he joined)
- 20:09, 12 April 2023 User account Roark talk contribs was created
- 19:00, 11 April 2023 Barreraz talk contribs created page File:EBeam4 Operating Instructions 4-7-2023.pdf (Updated Operating Instructions for EBeam4)
- 19:00, 11 April 2023 Barreraz talk contribs uploaded File:EBeam4 Operating Instructions 4-7-2023.pdf (Updated Operating Instructions for EBeam4)
- 22:34, 4 April 2023 John d talk contribs deleted page Field Emission SEM 1 (FEI Sirion) (Equipment is not available anymore: content was: "{{tool2|{{PAGENAME}} |picture=SEM1.jpg |type = Inspection, Test and Characterization |super= Aidan Hopkins |super2= Bill Mitchell |location=Bay 1 |description = FEI Thermal Field Emission SEM Sirion with EDAX Falcon EDX system |manufacturer = FEI |materials = |toolid=4 }} =About= This system is a tri-use FESEM imaging and inspection system, EDX elemental analysis system, and small-area electron beam lithography system. The system uses a ther...)
- 22:34, 4 April 2023 John d talk contribs deleted page Field Emission SEM 1 (Equipment is not available anymore)
- 17:07, 2 April 2023 John d talk contribs created page File:Vented font DDJ.gds (Vented Font - a font good for liftoff (no enclosed holes), GDS CAD file)
- 17:07, 2 April 2023 John d talk contribs uploaded File:Vented font DDJ.gds (Vented Font - a font good for liftoff (no enclosed holes), GDS CAD file)
- 20:03, 21 March 2023 John d talk contribs created page File:Surfscan P1 SiN 221208Z5G4 after.jpg
- 20:03, 21 March 2023 John d talk contribs uploaded File:Surfscan P1 SiN 221208Z5G4 after.jpg
- 19:59, 21 March 2023 John d talk contribs created page File:Surfscan G4 before example - P1 230317E7G4 before.jpg