Lithography Recipes: Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
m →Lift-Off Techniques: deleted redlink
Line 303: Line 303:
==Lift-Off Techniques==
==Lift-Off Techniques==


*{{fl|Liftoff-Techniques.pdf|Description/Tutorial}}
*{{fl|Liftoff-Techniques.pdf|Lift-Off Description/Tutorial}}
*[[Lift-Off Tutorial|Lift-Off Tutorial and Limits]]
**How it works, process limits and considerations for designing your process
**How it works, process limits and considerations for designing your process
*{{fl|Bi-LayerContactprocesswithPMGI.pdf|I-Line Lift-Off: Bi-Layer Process with PMGI Underlayer and Contact Aligner}}
*{{fl|Bi-LayerContactprocesswithPMGI.pdf|I-Line Lift-Off: Bi-Layer Process with PMGI Underlayer and Contact Aligner}}

Revision as of 21:05, 17 June 2020

General Information

This page contains information and links to recipes/datasheets spin-coated materials used in the facility.

Table of Contents
  • Underlayers
    • These are used beneath resists for both adhesive purposes and to enable bi-layer lift-off profiles for use with photoresist.
    • Datasheets are provided.
  • Lift-Off Techniques
    • Verified Recipes for lift-off using various photolith. tools
    • General educational description of this technique and it's limitations/considerations.
  • Holography
    • For 1-D and 2-D gratings with 220nm nominal period, available on substrates up to 1 inch square.
    • Recipes for silicon substrates are provided, and have been translated to other substrates by users.
  • Anti-Reflection Coatings:
    • The Photoresist Recipes section contains recipes using these materials.
    • Bottom Anti-Reflection Coatings (BARC) are used in the stepper systems, underneath the resists to eliminate substrate reflections that can affect resolution and repeatability for small, near resolution limited, feature sizes.
    • Datasheets are provided for reference on use of the materials.
  • Contrast Enhancement Materials (CEM)
    • The Photoresist Recipes section contains recipes using these materials.
    • Used for resolution enhancement. Not for use in contact aligners, typically used on I-Line Steppers.
    • Datasheets provided with usage info.
  • Adhesion Promoters
    • These are used to improve wetting of photoresists to your substrate.
    • Datasheets are provided on use of these materials.

Photolithography Recipes

  • R = Recipe is available. Clicking this link will take you to the recipe.
  • A = Material is available for use, but no recipes are provided.


Photolithography Recipes

Contact Aligner Recipes Steppers Recipes
Positive Resists SUSS MJB-3 SUSS MA-6 Stepper 1
(GCA 6300)
Stepper 2
(AutoStep 200)
Stepper 3
(ASML DUV)
MLA150
(Heidelberg)
AZ4110 R1 R1 A A
AZ4210 R1 R1 A A
AZ4330RS R1 R1 A A
OCG 825-35CS A A A A
SPR 950-0.8 A A A A
SPR 955 CM-0.9 A R1 R1 R1
SPR 955 CM-1.8 A A R1 R1
SPR 220-3.0 R1 R1 R1 R1
SPR 220-7.0 R1 R1 R1 R1
THMR-IP3600 HP D

A A
UV6-0.8 R1
UV210-0.3 R1
UV26-2.5 A
Negative Resists SUSS MJB-3 SUSS MA-6 Stepper 1
(GCA 6300)
Stepper 2
(AutoStep 200)
Stepper 3
(ASML DUV)
MLA150
(Heidelberg)
AZ5214-EIR R1 R1 R1 R1
AZnLOF 2020 R1 R1 R1 R1
AZnLOF 2035 A A A A
AZnLOF 2070 A A A A
AZnLOF 5510 A A R1 R1
UVN30-0.8 R1
SU-8 2005,2010, 2015 A R1 A A
SU-8 2075 A A A A
NR9-1000,3000,6000PY R1 R1 A R1
Anti-Reflection Coatings SUSS MJB-3 SUSS MA-6 Stepper 1
(GCA 6300)
Stepper 2
(AutoStep 200)
Stepper 3
(ASML DUV)
MLA150
(Heidelberg)
DUV42-P R1
DS-K101-304 R1
SUSS MJB-3 SUSS MA-6 Stepper 1
(GCA 6300)
Stepper 2
(AutoStep 200)
Stepper 3
(ASML DUV)
MLA150
(Heidelberg)

E-Beam Lithography Recipes

  • Under Development.

Automated Coat/Develop System Recipes (S-Cubed Flexi)

Recipes pre-loaded on the S-Cubed Flexi automated coat/bake/develop system. Only staff may write new recipes, contact the tool supervisor for more info.

To Be Added

Nanoimprinting Recipes

Holography Recipes

Low-K Spin-On Dielectric Recipes

Lift-Off Techniques

Chemicals Stocked + Datasheets

The following is a list of the lithography chemicals we stock in the lab, with links to the datasheets for each. The datasheets will often have important processing info such as spin-speed vs. thickness curves, typical process parameters, bake temps/times etc.

Positive Photoresists

i-line and broadband

DUV-248nm


Negative Photoresists

i-line and broadband

DUV-248nm


Underlayers


E-beam resists


Nanoimprinting
Contrast Enhancement Materials


Anti-Reflection Coatings


Adhesion Promoters


Spin-On Dielectrics

Low-K Spin-On Dielectrics such as Benzocyclobutane and Spin-on Glass


Developers


Photoresist Removers