Thermal Processing Recipes

From UCSB Nanofab Wiki
Revision as of 06:56, 16 November 2017 by John d (talk | contribs) (added some text and links to tools.)
Jump to navigation Jump to search

Thermal Oxidation of Silicon

Online calculators for thermal oxidation can be used to estimate the oxidation time for a desired oxidation thickness.

Please see Calculators + Utilities page for links to these oxidation calculators.

Thermal oxidation recipes for Wet (H2O vapor) and Dry (O2 gas) oxidation up to 1050°C are available on the TyStar 8300 system.

Wafer Substrate Bonding

Numerous research groups perform wafer bonding using either the Suss Wafer Bonder or a custom graphite fixture and any one of numerous ovens, such as the N2-purged Wafer Bonding Furnace (with glove box) or N2-purged Blue M oven.

The EVG Plasma Activation system and Goniometer allow for surface prep/inspection prior to bonding.