Difference between revisions of "Thermal Processing Recipes"
Jump to navigation
Jump to search
(added some text and links to tools.) |
m (minor grammar) |
||
Line 2: | Line 2: | ||
Online calculators for thermal oxidation can be used to estimate the oxidation time for a desired oxidation thickness. |
Online calculators for thermal oxidation can be used to estimate the oxidation time for a desired oxidation thickness. |
||
− | Please see [[Calculators + Utilities]] page for links to these oxidation calculators. |
+ | Please see the [[Calculators + Utilities]] page for links to these oxidation calculators. |
Thermal oxidation recipes for Wet (H2O vapor) and Dry (O2 gas) oxidation up to 1050°C are available on the [[Tube Furnace (Tystar 8300)|TyStar 8300 system]]. |
Thermal oxidation recipes for Wet (H2O vapor) and Dry (O2 gas) oxidation up to 1050°C are available on the [[Tube Furnace (Tystar 8300)|TyStar 8300 system]]. |
Revision as of 23:56, 15 November 2017
Thermal Oxidation of Silicon
Online calculators for thermal oxidation can be used to estimate the oxidation time for a desired oxidation thickness.
Please see the Calculators + Utilities page for links to these oxidation calculators.
Thermal oxidation recipes for Wet (H2O vapor) and Dry (O2 gas) oxidation up to 1050°C are available on the TyStar 8300 system.
Wafer Substrate Bonding
Numerous research groups perform wafer bonding using either the Suss Wafer Bonder or a custom graphite fixture and any one of numerous ovens, such as the N2-purged Wafer Bonding Furnace (with glove box) or N2-purged Blue M oven.
The EVG Plasma Activation system and Goniometer allow for surface prep/inspection prior to bonding.