Template:News - Older Articles: Difference between revisions
moved old articles to here |
pasted old articles |
||
| Line 1: | Line 1: | ||
===DREAMS Hub awarded 2 projects in GaN and 5G/6G technologies=== |
|||
[https://viterbischool.usc.edu/news/2024/09/usc-viterbi-led-ca-dreams-hub-is-awarded-31-9-million-in-funding-under-the-microelectronics-commons/ CA DREAMS Hub is awarded $31.9 million in funding under the Microelectronics Commons] - |
|||
* $16.2 Million to develop advanced gallium nitride (GaN) semiconductor technologies, with partners including USC, Northrop Grumman, Teledyne Technologies, HRL Laboratories, PseudolithIC, Monde Wireless Inc., Transphorm, UCLA and UC Santa Barbara. |
|||
* $15.7 Million in Funding for 5G/6G millimeter-wave Phased-Array Prototypes, with team USC, Northrop Grumman, HRL Laboratories, Teledyne, Caltech, UCLA, UC Santa Barbara, UC San Diego, Vorago, Global Foundries. |
|||
// [[User:John_d|Demis D. John]] 16:32, 23 September 2024 (PDT) |
|||
===NSF-ATE Award for SBCC and UCSB: New Semiconductor Pathway=== |
|||
The UCSB NanoFab and CNSI were recently awarded a project by NSF-ATE to build a semiconductor pathway (associates degree or certificate) at Santa Barbara City College, utilizing UCSB Cleanrooms. The project "[https://www.nsf.gov/awardsearch/showAward?AWD_ID=2400982 Expansion of CCPRIME: Central Coast Partnership for Regional Industry-Focused Micro/Nanotechnology Education]" is one of 6 projects funded by an [https://new.nsf.gov/news/nsf-invests-76m-educational-projects-build-skilled Intel-NSF partnership.] The project builds on the existing "[https://nanofab.ucsb.edu/workforce#bootcamps Cleanroom Bootcamps]" already being run twice a year in the [https://www.cnsi.ucsb.edu/facilities/quantum-structures CNSI QSF cleanroom]. // [[User:John_d|Demis D. John]] 13:15, 14 August 2024 (PDT) |
|||
===CHIPS Act Award Announced to USC and UCSB NanoFab=== |
|||
[https://carbajal.house.gov/news/documentsingle.aspx?DocumentID=1672 U.S. Congressman Salud Carbajal congratulates UCSB and the NanoFab] on receiving a [https://www.nist.gov/chips CHIPS & Science Act] award, as part of the [https://microelectronicscommons.org/ California DREAMS Hub (Microelectronics Commons) led by USC]. |
|||
-- [[User:John d|Demis]] 12:06, 4 October 2023 (PDT) |
|||
=== RIE#3 Removed === |
|||
We have removed [[RIE_3_(MRC)|RIE#3]] from the Nanofab, it has gone to the [https://www.ece.ucsb.edu/department-resources/electronics-shop/tcr Teaching Cleanroom]. All user's processes have been transferred to the [[Fluorine_ICP_Etcher_(PlasmaTherm/SLR_Fluorine_ICP)|Fluorine ICP Etcher]]. // [[User:John_d|Demis D. John]] 15:58, 6 August 2024 (PDT) |
|||
=== NanoFab staff awarded Goleta's Innovator of the Year 2023 === |
|||
NanoFab staff member [[Demis D. John]] has been awarded the ''City of Goleta's "Innovator of the Year"'' for 2023! The award stems from the UCSB Nanofab's impact on the communities of Santa Barbara County and surrounding regions, in enabling cutting edge technology companies to thrive, which also enables many local careers in advanced high-tech. See the [https://sbscchamber.com/goletas-finest-2023-award-recipients-announced/ full announcement by the Santa Barbara South Coast Chamber of Commerce]. // [[User:John d|Demis D. John]] 13:58, 7 November 2023 (PST) |
|||
=== NanoFab Featured in Regional Tech Videos === |
|||
The UCSB NanoFab is showcased as a driver of innovation and enabler of the regional high-tech industry. |
|||
See the videos here: |
|||
{| class="wikitable" |
|||
|[https://fast.wistia.net/embed/iframe/l46hsnwg4b?controlsVisibleOnLoad=true&muted=0&playerColor©LinkAndThumbnailEnabled=false '''''Santa Barbara County: This is TechTopia'''''] [[File:Techtopia_Vid_-_Thumbnail_PlayButton.jpg|none|300x300px|link=https://fast.wistia.net/embed/iframe/l46hsnwg4b?controlsVisibleOnLoad=true&muted=0&playerColor©LinkAndThumbnailEnabled=false]] |
|||
|[https://www.youtube.com/watch?v=op746os6eRI '''''UCSB NanoFab: An Innovation Center'''''] [[File:NanoFab_COE_Engineering_Vid_-_thumbnail_2_crop.jpg|none|300x300px|link=https://www.youtube.com/watch?v=op746os6eRI]] |
|||
|} |
|||
// [[User:John d|John d]] 09:26, 1 November 2023 (PST) |
|||
=== CHIPS Act Award Announced to USC and UCSB NanoFab === |
=== CHIPS Act Award Announced to USC and UCSB NanoFab === |
||
[https://carbajal.house.gov/news/documentsingle.aspx?DocumentID=1672 U.S. Congressman Salud Carbajal congratulates UCSB and the NanoFab] on receiving a [https://www.nist.gov/chips CHIPS & Science Act] award, as part of the [https://microelectronicscommons.org/ California DREAMS Hub (Microelectronics Commons) led by USC]. |
[https://carbajal.house.gov/news/documentsingle.aspx?DocumentID=1672 U.S. Congressman Salud Carbajal congratulates UCSB and the NanoFab] on receiving a [https://www.nist.gov/chips CHIPS & Science Act] award, as part of the [https://microelectronicscommons.org/ California DREAMS Hub (Microelectronics Commons) led by USC]. |
||
Latest revision as of 19:57, 3 October 2026
DREAMS Hub awarded 2 projects in GaN and 5G/6G technologies
CA DREAMS Hub is awarded $31.9 million in funding under the Microelectronics Commons -
- $16.2 Million to develop advanced gallium nitride (GaN) semiconductor technologies, with partners including USC, Northrop Grumman, Teledyne Technologies, HRL Laboratories, PseudolithIC, Monde Wireless Inc., Transphorm, UCLA and UC Santa Barbara.
- $15.7 Million in Funding for 5G/6G millimeter-wave Phased-Array Prototypes, with team USC, Northrop Grumman, HRL Laboratories, Teledyne, Caltech, UCLA, UC Santa Barbara, UC San Diego, Vorago, Global Foundries.
// Demis D. John 16:32, 23 September 2024 (PDT)
NSF-ATE Award for SBCC and UCSB: New Semiconductor Pathway
The UCSB NanoFab and CNSI were recently awarded a project by NSF-ATE to build a semiconductor pathway (associates degree or certificate) at Santa Barbara City College, utilizing UCSB Cleanrooms. The project "Expansion of CCPRIME: Central Coast Partnership for Regional Industry-Focused Micro/Nanotechnology Education" is one of 6 projects funded by an Intel-NSF partnership. The project builds on the existing "Cleanroom Bootcamps" already being run twice a year in the CNSI QSF cleanroom. // Demis D. John 13:15, 14 August 2024 (PDT)
CHIPS Act Award Announced to USC and UCSB NanoFab
U.S. Congressman Salud Carbajal congratulates UCSB and the NanoFab on receiving a CHIPS & Science Act award, as part of the California DREAMS Hub (Microelectronics Commons) led by USC. -- Demis 12:06, 4 October 2023 (PDT)
RIE#3 Removed
We have removed RIE#3 from the Nanofab, it has gone to the Teaching Cleanroom. All user's processes have been transferred to the Fluorine ICP Etcher. // Demis D. John 15:58, 6 August 2024 (PDT)
NanoFab staff awarded Goleta's Innovator of the Year 2023
NanoFab staff member Demis D. John has been awarded the City of Goleta's "Innovator of the Year" for 2023! The award stems from the UCSB Nanofab's impact on the communities of Santa Barbara County and surrounding regions, in enabling cutting edge technology companies to thrive, which also enables many local careers in advanced high-tech. See the full announcement by the Santa Barbara South Coast Chamber of Commerce. // Demis D. John 13:58, 7 November 2023 (PST)
NanoFab Featured in Regional Tech Videos
The UCSB NanoFab is showcased as a driver of innovation and enabler of the regional high-tech industry.
See the videos here:
| Santa Barbara County: This is TechTopia |
UCSB NanoFab: An Innovation Center |
// John d 09:26, 1 November 2023 (PST)
CHIPS Act Award Announced to USC and UCSB NanoFab
U.S. Congressman Salud Carbajal congratulates UCSB and the NanoFab on receiving a CHIPS & Science Act award, as part of the California DREAMS Hub (Microelectronics Commons) led by USC. // Demis 12:06, 4 October 2023 (PDT)
JEOL SEM's Installed
Both SEM's have been replaced with new JEOL SEM's #1 and SEM #2. SEM#1 has the NABITY lithography system installed, and SEM #2 has always-on EDAX elemental analysis. Contact the supervisor, Aidan Hopkins, for more information. // John d 18:31, 20 September 2023 (PDT)
Wide FOV Microscope Installed
We have installed an AmScope stereo microscope in Bay 4 for wide field-of-view digital imaging/capture, with >2cm of FOV currently available. Wiki page here: AmScope Wide Field of View Stereoscope // John d 14:52, 19 April 2023 (PDT)
Loomis Scribe & Break installed
We have installed a new Loomis LSD-155LT Automated Scribe & Break Cleaving tool in the Back-End Processing lab. Qualifications are underway. Contact supervisor, Aidan Hopkins, for more information. // John d 09:41, 16 April 2023 (PDT)
Dektak XT installed
We have replaced the old Dektak 6M with a new Dektak XT profilometer. This tool will provide robust, fast metrology for rapid in-process topography inspection. // John d 10:41, 25 January 2023 (PST)
New Process Control data tables
We have added "Process Control Data" - data on deposition/etch repeatability - to a number of our highest used etchers and deposition tools. The datasheets are linked in multiple places, mainly on the Recipes pages for each tool, or on the general Recipes pages for Deposition Recipes or Etch Recipes. // John d 16:07, 5 January 2023 (PST)
Oxford PlasmaPro ICP Etcher installed
We have a new ICP etcher in Bay 2: Oxford_ICP_Etcher_(PlasmaPro_100_Cobra)
The tool has been qualified for InP Ridge and InGaAsP Grating etches, and is intended for III-V etching in general (GaAs, GaN, GaSb etc.)
In addition, the tool is capable of Atomic Layer Etching on various materials. Contact the supervisor for training. // John d 11:27, 29 September 2021 (PDT)
SiO2 etching, High-Aspect Ratio
Dr. Bill Mitchell recently published an article detailing high-aspect ratio SiO2 etching (JVST-A, May 2021) in the Plasma-Therm Fluorine ICP etcher, using a novel Ruthenium Hard Mask.
Ruthenium can be deposited using the Oxford ALD or AJA Sputter and etched in one of the Panasonic ICP's.
You can find a full process flow at the FL-ICP's Recipe Page, in this case using a Sputtered Ru hard mask and I-line stepper lithography. // John d 08:05, 27 May 2021 (PDT)
Wafer Polisher available
We have added an Allied Wafer Polish tool to our equipment list. Contact Bill_Millerski for more information. // John d 16:49, 10 May 2021 (PDT)
Digital Microscope: Olympus DSX-1000
You'll see a new digital microscope in Bay 4/Metrology, that's our new Olympus DSX-1000. We are currently developing procedures, keep an eye out for training emails. // John d 13:49, 8 April 2021 (PDT)
Raith Velion: FIB/SEM Installation
We have installed a new state-of-the-art focused ion beam/electron beam tool in Bay 1. The Raith Velion enables synchronized interferometric stage, Focused-ion Beam Lithography with ~10nm features or less, live SEM during writing, and Electron-Beam Lithography.
Learn more about the tool's capabilities at the Raith website:
- Raith Products: Velion.
- VIDEO: Synchronized FIB beam + Laser Interferometric Stage write, with live SEM
Tool qualification is currently underway. Dr. Dan Read is the resident expert on this new tool.
// John d 06:53, 30 November 2020 (PST)
Heidelberg MLA-150: Delivery Scheduled for Sept.
Our Heidelberg Maskless Aligner (MLA150) will be installed the week of September 21st 2020! This tool enables flexible I-Line lithography, in which a user can align to arbitrary features (eg. 2D materials, quantum dots), upload a CAD file to write a pattern without ordering a mask plate, grey-scale lithography and continuous auto-focus on non-planar substrates.
Learn more about the tool at the Heidelberg Instruments website:
// John d 11:41, 14 September 2020 (PDT)
TechTalk: Dr. Renan Moreira & Grégoire Coiffard
Tech Talks on Thurs Dec 5th, in ESB room 1001 (click for more info):
12n: Dr. Renan Moreira, ULL Technologies: “Ultra-low loss photonic integrated circuits based on Si3N4 waveguides”
1245pm: Grégoire Coiffard, Mazin Group, Physics Dept. UCSB, “The fabrication of 20,000 pixel kinetic inductance detector arrays for near-IR to visible astronomy” // John d 11:03, 5 December 2019 (PDT)
New Plasma Asher Installation
A new YES EcoClean Plasma Strip/Descum System is being installed, for controlled photoresist etching & residue stripping. We will make an announcement when the system has been qualified and is ready for use. // John d 11:03, 7 August 2019 (PDT)
Rapid Thermal Annealer Installed
We are installing and qualifying a new SSI Solaris 150 Rapid Thermal Processor. We will make an announcement when the system is ready and trainings are scheduled. See the SSI RTP Wiki Page here. // John d 12:03, 28 May 2019 (PDT)
S-Cubed Spin/Coat/Dev Station Installation
We are currently in the process of installing a Cube system for automated Spin Coating, Baking, Developing and Edge-Bead Removal on 4-inch and 6-inch wafers. Initially this tool will be solely purposed for Staff and the use of the sponsor, primarily for ASML DUV Stepper wafer prep. As procedures are developed, the system will be opened up for use by all ASML Stepper users, and may eventually be opened for I-Line stepper use as well. // John d 12:10, 20 February 2019 (PST)
Filmetrics Optical Measurement Systems
A Filmetrics F10-RT for optical reflection/transmission spectra, and a Filmetrics F50 thin-film wafer-mapping system have been installed. Contact Ning Cao for more info. // John d 15:24, 12 December 2018 (PST)
KLA Tencor Profilometer Installed
We have installed a new KLA Tencor Stylus Profilometer, that has been installed in Bay 4. Contact Brian Lingg for training. // John d 17:28, 12 September 2018 (PDT)
Laser Endpoint Monitors
We've installed new Intellemetrics LEP500 Laser Endpoint Detection monitoring on the DSEiii & ICP#2 & ICP#1 etchers. This allows you to terminate your etch at a calibrated/modeled distance into a layer, and removes the need to calibrate etch rates for most processes. // John d 09:26, 17 July 2018 (PDT)
Metal Processes on the Atomic Layer Deposition
We now have Ruthenium (Ru) and Platinum (Pt) metal depositions developed on the Oxford FlexAL ALD tool. See the Atomic Layer Deposition: Recipes page or contact Bill Mitchell for more information. // Posted: 16:07, 01 June 2017 (PST)
New Deep Silicon Etcher Online
A new Plasma-Therm Versaline DSE III DRIE etcher has been qualified for bosch etch and single-step etches, and is available for use. The new tool features much higher silicon etch rates, improved uniformity, and allows for photoresist up to the edges of the wafer. An Intellemetrics LEP500 laser end point monitor has also been installed on the system. // Posted: 22:16, 27 November 2017 (PST)
2016 Survey Results
See the May 2016 User Survey Results. // Posted: 12:00, 01 May 2016 (PST)
CAIBE Ion Mill Available
The CAIBE (Oxford Ion Mill) is up and running! Contact Brian Lingg for more information. // Posted: 12:00, 01 July 2015 (PST)
NanoFiles SFTP Online
Files generated with Nanofab tools (SEM images, AFM profiles, etc.) are now available on the nanofab SFTP server. Please check SignupMonkey for details. // Posted: 12:00, 07 July 2013 (PST)