User contributions for John d
Jump to navigation
Jump to search
20 March 2023
- 23:2423:24, 20 March 2023 diff hist +122 Calculators + Utilities →KLayout: like to U. waterloo KLayout vids Tag: Visual edit
- 23:0523:05, 20 March 2023 diff hist +1,728 N Oxford Etcher - Sample Size Effect on Etch Rate pasted from old Process Control Dataa: Oxford_ICP_Etcher_-_Process_Control_Data current Tag: Visual edit: Switched
- 23:0523:05, 20 March 2023 diff hist +179 ICP Etching Recipes →Process Control Data (Oxford ICP Etcher): link to Sample Size effect on ER Tag: Visual edit
- 23:0223:02, 20 March 2023 diff hist +41 m Template:News link to all data
- 18:0418:04, 20 March 2023 diff hist +3 Template:Announcements corected SEM #2 --> SEM#1
19 March 2023
- 05:0105:01, 19 March 2023 diff hist +27 N User:Mehalana v redirects to Vraj's correct staff page current Tags: New redirect Visual edit: Switched
16 March 2023
- 17:2717:27, 16 March 2023 diff hist −8 Stepper 3 (ASML DUV) →Operating Procedures: moved training procedure above Tag: Visual edit
15 March 2023
- 19:2219:22, 15 March 2023 diff hist +19 GCA 6300 Mask Making Guidance link to Autostep 200 mask page
- 19:2119:21, 15 March 2023 diff hist +97 GCA 6300 Mask Making Guidance No edit summary
- 19:1619:16, 15 March 2023 diff hist 0 m Stepper 2 (AutoStep 200) →Process Information Tag: Visual edit
- 19:1619:16, 15 March 2023 diff hist +25 m Stepper 2 (AutoStep 200) →Process Information Tag: Visual edit
- 19:1519:15, 15 March 2023 diff hist +180 Stepper 2 (AutoStep 200) copied Mask making link to SOP section as well, minor formatting elsewhere. Tag: Visual edit
- 17:3117:31, 15 March 2023 diff hist +2,035 Autostep 200 Mask Making Guidance addded Submission Details section Tag: Visual edit
13 March 2023
- 23:2323:23, 13 March 2023 diff hist 0 File:Single centered mask-Piece 2nd litho AUTOSTEP 200.pptx John d uploaded a new version of File:Single centered mask-Piece 2nd litho AUTOSTEP 200.pptx current
10 March 2023
- 21:0921:09, 10 March 2023 diff hist +643 Stepper Recipes →Stepper 3 (ASML DUV): added Process Control Data section
- 21:0721:07, 10 March 2023 diff hist +45 m Process Group - Process Control Data Litho to Top of page, link to ASML recipes page
- 21:0421:04, 10 March 2023 diff hist +738 Process Group - Process Control Data New Litho section + Stepper3 ASML section with links to process control data Tag: Visual edit: Switched
- 21:0121:01, 10 March 2023 diff hist +1,321 Stepper 3 (ASML DUV) link to Process Control Data Tag: Visual edit
5 March 2023
- 22:3622:36, 5 March 2023 diff hist +114 XeF2 Etch (Xetch) Link to recipes oage Tag: Visual edit
26 February 2023
- 07:1707:17, 26 February 2023 diff hist +14 Template:Announcements →Flip-Chip Bonder repair
- 03:1203:12, 26 February 2023 diff hist −16 Template:Announcements FCB update
25 February 2023
- 17:1717:17, 25 February 2023 diff hist +8 m Step Profilometer (DektakXT) added date of replacement Tag: Visual edit
23 February 2023
- 23:0023:00, 23 February 2023 diff hist +797 PECVD Recipes →ICP-PECVD (Unaxis VLR): cleaned up process control section, and added 800nm max SiO2 thickness before cleaning Tag: Visual edit
21 February 2023
- 22:0122:01, 21 February 2023 diff hist −51 Probe Station: I-V Curves with Keithley 2400 and Python Script anaconda inzstruction Tag: Visual edit
20 February 2023
- 16:5316:53, 20 February 2023 diff hist +56 ICP Etching Recipes →Process Control Data (Oxford ICP Etcher): linked to new google sheets data Tag: Visual edit
17 February 2023
- 04:4504:45, 17 February 2023 diff hist +37 Photolithography - Manual Edge-Bead Removal Techniques →Lithographic Edge Bead Removal: link to DUV FLood exposure Tag: Visual edit
- 04:4304:43, 17 February 2023 diff hist +2 m Lithography Recipes fixed link Tag: Visual edit
- 04:4204:42, 17 February 2023 diff hist +2 m Lithography Recipes remove TOC again
- 04:4204:42, 17 February 2023 diff hist +36 Lithography Recipes →General Photolithography Techniques: made each section a linkable header level Tag: Visual edit
- 04:4004:40, 17 February 2023 diff hist −2 m Lithography Recipes add TOC to get header link
14 February 2023
- 19:3619:36, 14 February 2023 diff hist +995 Frequently Asked Questions →General NanoFab Questions: added "what supplies do i need to bring?" Tag: Visual edit
- 19:2119:21, 14 February 2023 diff hist −1 m Template:Announcements No edit summary
- 01:3101:31, 14 February 2023 diff hist −86 Template:Announcements FCB update
13 February 2023
- 17:3517:35, 13 February 2023 diff hist +323 Template:Announcements Unaxis Etch Down
- 17:3417:34, 13 February 2023 diff hist +121 Template:Announcements FCB update
10 February 2023
- 20:2320:23, 10 February 2023 diff hist +168 Probe Station & Curve Tracer →Operation Procedures & Manuals: linked to probe station usage rules current Tag: Visual edit
- 16:2816:28, 10 February 2023 diff hist −9 m Tool List →Electrical Analysis: fix QFI link Tag: Visual edit
8 February 2023
- 07:2507:25, 8 February 2023 diff hist +247 Maskless Aligner (Heidelberg MLA150) →Documentation: link to FEM tips Tag: Visual edit
7 February 2023
- 23:3223:32, 7 February 2023 diff hist +250 MLA150 - Design Guidelines →Greyscale Lithography: addded more info Tag: Visual edit
- 23:2823:28, 7 February 2023 diff hist +833 ASML Stepper 3 Standard Operating Procedure →Running a focus and/or exposure matrix: added "general process" for FEMs Tag: Visual edit
- 18:0818:08, 7 February 2023 diff hist +6 Template:Announcements updated Dektak XT, link for training available
- 18:0618:06, 7 February 2023 diff hist −54 Step Profilometer (DektakXT) updated that tool is availabel for training. Tag: Visual edit
6 February 2023
- 18:3718:37, 6 February 2023 diff hist +202 Template:Announcements added back the "ENDFEED" lines and updated comment to indicate not to delete this.
1 February 2023
- 18:2418:24, 1 February 2023 diff hist −28 m Foong Fatt No edit summary current
- 18:2418:24, 1 February 2023 diff hist −8 m Foong Fatt No edit summary
- 18:1918:19, 1 February 2023 diff hist +296 N Foong Fatt initial page copied from Demis D John Tag: Visual edit: Switched
- 18:1718:17, 1 February 2023 diff hist −7 Staff List Afdded Foong Tag: Visual edit
30 January 2023
- 21:5621:56, 30 January 2023 diff hist +200 ICP Etching Recipes →PlasmaTherm/SLR Fluorine Etcher: added recipe tips, RF 1/RF 2/ignition tips. Tag: Visual edit
- 14:4914:49, 30 January 2023 diff hist −4 Nanofab Job Postings deleted Process Engineer, added Undergrad process technician Tag: Visual edit
- 03:0403:04, 30 January 2023 diff hist +314 Template:Announcements jeol sem down