Atomic Layer Deposition (Oxford FlexAL)
Al2O3 deposition (ALD)
AlN deposition (ALD)
HfO2 deposition (ALD)
SiO2 deposition (ALD)
ZrO2 deposition (ALD)
TiO2 deposition (ALD)
TiO2 recipe WJM_TDMAT_H2O_r2 water dose 1s (pdf file to be added), at 200C, gives grow rate 0.11 nm/cy as measured by ellipsometer