Recent changes

Jump to navigation Jump to search

Track the most recent changes to the wiki on this page.

Recent changes options Below are the changes since 12 July 2024, 16:19 (up to 50 shown). (Reset date selection)
Show last 50 | 100 | 250 | 500 changes in last 1 | 3 | 7 | 14 | 30 days
Hide registered users | Hide anonymous users | Show my edits | Show bots | Hide minor edits
Show new changes starting from 10:07, 6 August 2024
   
List of abbreviations:
N
This edit created a new page (also see list of new pages)
m
This is a minor edit
b
This edit was performed by a bot
(±123)
The page size changed by this number of bytes

5 August 2024

     10:16  Vacuum Deposition Recipes‎‎ 5 changes history +3,717 [Noahdutra‎ (5×)]
     
10:16 (cur | prev) +2,866 Noahdutra talk contribs added Ebeams rankings Tag: Visual edit
     
09:55 (cur | prev) -30 Noahdutra talk contribs Tag: Visual edit
     
09:54 (cur | prev) -47 Noahdutra talk contribs Tag: Visual edit
     
09:53 (cur | prev) +16 Noahdutra talk contribs Tag: Visual edit
     
09:52 (cur | prev) +912 Noahdutra talk contribs added process ranking table Tag: Visual edit

3 August 2024

N    18:05  Processing - How Do I…? diffhist +538 John d talk contribs initial holders Tag: Visual edit

1 August 2024

     17:21  Hummer SEM Sample Coater - Techniques to reduce charging in SEMs diffhist +272 John d talk contribs link to Hummer tool page Tag: Visual edit
     17:17  SEM Sample Coater (Hummer)‎‎ 2 changes history +38 [John d‎ (2×)]
     
17:17 (cur | prev) +1 John d talk contribs →‎Operating Procedures: fixed bullet points, listed approx film thickness Tag: Visual edit
     
17:17 (cur | prev) +37 John d talk contribs →‎About Tag: Visual edit
     17:16  SEM 1 (JEOL IT800SHL) diffhist +70 John d talk contribs →‎Operating Procedures: link to hummer techniques Tag: Visual edit

31 July 2024

     18:52  Template:Announcements diffhist +372 Mehalana v talk contribs
     17:46  Lift-Off with DUV Imaging + PMGI Underlayer diffhist +148 John d talk contribs →‎Suggested Process for Liftoff: added N2 dry step Tag: Visual edit
     14:13  Vacuum Deposition Recipes‎‎ 6 changes history -522 [Ffoong‎ (6×)]
     
14:13 (cur | prev) -20 Ffoong talk contribs Correct the links for UNAXIS PECVD Tag: Visual edit
     
14:12 (cur | prev) -10 Ffoong talk contribs Tag: Visual edit
     
14:11 (cur | prev) +4 Ffoong talk contribs Add R level for UNAXIS PECVD Tag: Visual edit
     
13:39 (cur | prev) -20 Ffoong talk contribs R5 on IBD Al2O3 Tag: Visual edit
     
13:38 (cur | prev) -504 Ffoong talk contribs Added R levels to IBD dep Tag: Visual edit
     
11:00 (cur | prev) +28 Ffoong talk contribs add R levels for ALD system Tag: Visual edit

30 July 2024

     15:34  Vacuum Deposition Recipes‎‎ 3 changes history +34 [Ffoong‎ (3×)]
     
15:34 (cur | prev) +15 Ffoong talk contribs change PECVD1 R levels and add links Tag: Visual edit
     
15:18 (cur | prev) +18 Ffoong talk contribs Changed PECVD2 levels and added proper internal links Tag: Visual edit
     
15:13 (cur | prev) +1 Ffoong talk contribs Changed Si in PECVD2 to R3 Tag: Visual edit
     15:04  Dry Etching Recipes‎‎ 5 changes history +98 [Ffoong‎; Noahdutra‎ (4×)]
     
15:04 (cur | prev) -1 Noahdutra talk contribs changed "Process Control Data" link at the top so it didn't have an "f" at the front of it. Tag: Visual edit
     
14:33 (cur | prev) 0 Ffoong talk contribs changed Al2O3 etch from R4 to R3 Tag: Visual edit
     
10:39 (cur | prev) +85 Noahdutra talk contribs corrected SiC for ICP2 so that it is R1 instead of R4, which was a mistake to ever put it at R4. Also added a link to GaAs etch on ICP2 Tag: Visual edit
     
10:36 (cur | prev) +83 Noahdutra talk contribs added link to Al etch Tag: Visual edit
     
10:35 (cur | prev) -69 Noahdutra talk contribs Did process rankings for ICP2, I also deleted a redundant row for Ru, there were two Ru rows Tag: Visual edit
     09:02  Laser Scanning Confocal M-scope (Olympus LEXT) diffhist +6 Hopkins a talk contribs →‎Offline software Tag: Visual edit
     09:00 Upload log Hopkins a talk contribs uploaded File:LEXT OLS4100 InstallManual Ver.3.1.8 offline.pdf(LEXT Offline software)
     08:10  Suss Aligners (SUSS MJB-3) diffhist +2 Sawyer l talk contribs
     08:10  Contact Aligner (SUSS MA-6) diffhist +2 Sawyer l talk contribs
     08:09  E-Beam 2 (Custom) diffhist +1 Sawyer l talk contribs
     08:06  ICP Etch 2 (Panasonic E626I) diffhist -6 Sawyer l talk contribs Tag: Visual edit: Switched

29 July 2024

     19:24  SEM 1 (JEOL IT800SHL) diffhist +108 John d talk contribs →‎Imaging: added minor descriptions on detector types Tag: Visual edit
 m   10:49  Dry Etching Recipes‎‎ 2 changes history +3 [Noahdutra‎; Ffoong‎]
 m   
10:49 (cur | prev) +3 Ffoong talk contribs Change A to R1 per Demis, almost all A have been done before. Tag: Visual edit
 m   
09:15 (cur | prev) 0 Noahdutra talk contribs →‎Dry Etching Tools/Materials Table: Added "R6" to the key/legend description Tag: Visual edit

26 July 2024

     16:26  Template:Announcements diffhist +20 Mehalana v talk contribs →‎Unaxis ICP-PECVD Update
     14:34  Dry Etching Recipes‎‎ 4 changes history +6 [Ffoong‎ (4×)]
     
14:34 (cur | prev) +5 Ffoong talk contribs Update OXFD recipe maturity levels Tag: Visual edit
     
14:24 (cur | prev) +1 Ffoong talk contribs input OXFD recipe maturity levels Tag: Visual edit
     
14:15 (cur | prev) +350 Ffoong talk contribs Undo revision 162126 by Ffoong (talk) Tag: Undo
     
14:05 (cur | prev) -350 Ffoong talk contribs update R levels to show maturity as defined in CA-Dreams Tag: Visual edit
     10:12  Laser Etch Monitoring‎‎ 2 changes history +910 [John d‎ (2×)]
     
10:12 (cur | prev) +121 John d talk contribs →‎Substrate Temperature Stabilization Tag: Visual edit
     
10:08 (cur | prev) +789 John d talk contribs added Joel's DSP Substrate trace example Tag: Visual edit
     10:06 Upload log John d talk contribs uploaded File:LaserMon - Temp Stabilize JoelGuo - 240725 noGas hold200C InPepi DSP.png

25 July 2024

     10:49  Template:Announcements‎‎ 3 changes history -107 [Mehalana v‎ (3×)]
     
10:49 (cur | prev) +1 Mehalana v talk contribs →‎Wafer Bonder, (Suss SB6-8E)
     
10:48 (cur | prev) +34 Mehalana v talk contribs →‎Unaxis ICP-PECVD Update
     
10:48 (cur | prev) -142 Mehalana v talk contribs

24 July 2024

     09:48  Dry Etching Recipes‎‎ 4 changes history +240 [John d‎ (4×)]
 m   
09:48 (cur | prev) +12 John d talk contribs →‎Process Ranking Table Tag: Visual edit
     
09:47 (cur | prev) +1 John d talk contribs fixed Pan1/2 links Tag: Visual edit
     
09:32 (cur | prev) +95 John d talk contribs →‎Process Ranking Table: minor updates to Process Maturity level Tag: Visual edit
     
09:30 (cur | prev) +132 John d talk contribs mention + link to table Key/Legend Tag: Visual edit